Electrospun of Bi 2 O 3 /WO 3 /PVA nanofibre mats with different WO 3 (0–35 wt%) filler loadings at constant 5 wt% Bi 2 O 3 filler loading or vice versa were fabricated for X-ray shielding purpose via an electrospinning process. The X-ray attenuation ability of the prepared electrospun Bi 2 O 3 /WO 3 /PVA nanofibre mats were compared at different X-ray energies (8.05–21.17 keV) using X-ray fluorescence (XRF) unit. The dispersion of Bi 2 O 3 /WO 3 fillers within PVA nanofibre mats were analysed using FESEM. Results revealed that the increment of Bi 2 O 3 /WO 3 filler loading within PVA nanofibre mats has enhanced the X-ray attenuation of the sample, but an opposite result was found for only the samples with (i) 20 wt% WO 3 filler loading at constant 5 wt% Bi 2 O 3 filler loading; and (ii) 30 wt% Bi 2 O 3 filler loading at constant 5 wt% WO 3 filler loading. The main reason for the deterioration of X-ray attenuation capability of these two samples might be due to the poor dispersions of the fillers found within the PVA nanofibre mats. Nevertheless, the outcome shows that the electrospun Bi 2 O 3 /WO 3 /PVA nanofibre mat with 35 wt% Bi 2 O 3 filler loading and constant 5 wt% WO 3 filler loading has the greatest X-ray attenuation ability compared to Bi 2 O 3 /WO 3 /PVA nanofibre mat for all filler loadings; thus it is recommended as X-ray shielding material candidate.
No takes yet. Share an insight, caveat, or question.
Ahmad et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: