To investigate an effect of internal hydrogen on mechanical properties of a new austenitic stainless steel “STH2” having a nominal composition of Fe-15%Cr-9%Mn-6%Ni-2.5%Cu-0.15~0.2%N, tensile tests and fatigue crack growth tests were conducted for the specimens containing around 80 ppm hydrogen charged by the exposure in 45 MPa hydrogen gas at 300˚C for 200 h and the ones heat treated in air with the same heat pattern.