Answers are grounded in this paper and cite their sources.
Fe 2 O 3 −Al 2 O 3 composite particles were synthesized by changing the sintering temperature in the range of 800−1370 °C under the conditions that the content of Fe 2 O 3 and the sintering time were given as 25 wt % and 10 h, respectively, and their applicability as a solid looping material of the chemical-loop combustor was discussed. Two solid solutions, Fe 2 O 3 (rich)−Al 2 O 3 (hematite(ss)) and Fe 2 O 3 −Al 2 O 3 (rich) (corundum(ss)), were formed at 1000 and 1250 °C, respectively, and the formation of these solid solutions was promoted by increasing the sintering temperature. Reduction tests of Fe 2 O 3 −Al 2 O 3 composite particles sintered in the temperature range of 1200−1370 °C were carried out by the pulse injection technique using hydrogen gas. In the low reduction range below 10%, Fe 2 O 3 in hematite(ss) was reduced to Fe 3 O 4, and that in corundum(ss) was not changed. Corundum(ss) is not useful for the reduction operation of the chemical-loop combustor. However, the mechanical strength of particles was improved by increasing the content of corundum(ss), which plays a role as binder between Fe 2 O 3 and Al 2 O 3 grains. For maintaining the durability and reactivity of particles, Fe 2 O 3 −Al 2 O 3 composite particles containing corundum(ss) to some extent, such as those sintered at 1320 °C, are suitable as a solid looping material of the chemical-loop combustor.
No takes yet. Share an insight, caveat, or question.
Ishida et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: