Answers are grounded in this paper and cite their sources.
Dextran ultra-fine nanofiber mats with uniform morphological appearance were fabricated using the electrospinning process. Increasing the solution concentration from 0.5 g.mL−1 to 0.9 g.mL−1 changed the fiber structure from coarse-beaded to a uniform beadless nanofiber mats. Additionally, reducing the feed rate from 1 mL.h−1 to 0.25 mL.h−1 with increasing the spinning distance from 150 to 170 mm generally led to a decrease in the diameters of the fibers. At the end; uniform dextran nanofibers with diameters ≈227 nm fabricated by the systematic modification of the electrospinning process. Crosslinked dextran nanofiber mats represent promising candidates for biomedical and tissue engineering.
No takes yet. Share an insight, caveat, or question.
Salimi‐Kenari et al. (2022) studied this question.