Copper was fixed in jute, coarse cotton, and woollen fabrics by dipping the test materials for two to five minutes in a 0.5% aqueous solution of dimethylglyoxime at 90° to 100 °C., and then immersing them in 5% copper acetate at room temperature for five minutes. The amount of fixed copper was varied by altering the strength of the copper solution. The treated fabrics were odourless, remained pliable, and were dyed a khaki colour. As determined by soil burial tests this treatment proved more effective than that with copper naphthenate for rotproofing purposes.