Answers are grounded in this paper and cite their sources.
We introduce low-loss amorphous titanium dioxide (TiO2) strip waveguides with sub-wavelength dimensions. The waveguides were fabricated by the combination of atomic layer deposition (ALD), electron beam lithography (EBL), and reactive ion etching (RIE). Propagation losses of the strip waveguides were found to be as low as 5.0 dB/cm at 1.55 μm wavelength. Those propagation losses are mostly due to the sidewall roughness of the waveguides that is caused by the lithography process. The propagation losses were further reduced by deposition, on the fabricated strip waveguides, of an additional layer of TiO2made by using ALD. A supplementary layer of TiO2with a thickness of 30 nm reduced the measured propagation losses from 5.0 ± 0.5 dB/cm to 2.4 ± 0.2 dB/cm at 1.55 μm wavelength. It is due to the fact that, after the redeposition process, the initial waveguide sidewall, i.e., the TiO 2/air interface, is virtually removed and the new sidewall has a reduced roughness.
No takes yet. Share an insight, caveat, or question.
Häyrinen et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: