Answers are grounded in this paper and cite their sources.
ZrO 2 powder was prepared by a sol–emulsion–gel method at temperatures below 140°C from ZrO(NO 3 ) 2 · n H 2 O. The asprepared powder was amorphous, but crystallized into the tetragonal structure by 600°C. The metastable tetragonal powder (600°C) was comprised of ultrafine 4‐ to 6‐nm size particles. On heat treatment, the tetragonal form completely transformed into the monoclinic state at 1100°C. Preliminary studies indicate good sinterability with densities greater than 94% at 1100°C and with a grain size of 0.25 μ.
No takes yet. Share an insight, caveat, or question.
Ramamurthi et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: