Answers are grounded in this paper and cite their sources.
Porous mullite (Al VI 2 (Al IV 2+2 x Si 2−2 x )O 10− x , where x ranges between 0.17 and 0.57) structures were fabricated by integrating sol–gel chemistry with digital light processing (DLP), enabling complex geometries with coupled micro‐ and macroporosity. The method uses a powder‐free, low‐viscosity photocurable sol–gel ink (0.012 Pa·s) based on molecularly mixed aluminum and silicon precursors, enabling high‐resolution printing and rapid photopolymerization (∼50% C = C conversion within 4 s). Supercritical drying (SCD) was applied after printing to suppress capillary stresses during solvent removal and preserve the printed geometry. After heat treatment at 1000°C, X‐ray diffraction confirmed mullite crystallization, despite this temperature being well below conventional powder‐sintering temperatures. The printed structures exhibit ∼74% total porosity, a dominant mesopore size of ∼12 nm, and a specific surface area of 64 ± 4 m 2 g − 1 . Thermal diffusivity increased only slightly from 0.292 to 0.322 mm 2 s − 1 between 300°C and 800°C, consistent with heat transport controlled by the porous ceramic framework. This powder‐free sol–gel/DLP route therefore provides a low‐temperature platform for fabricating lightweight, heat‐resistant mullite structures with controlled geometry and hierarchical porosity.
No takes yet. Share an insight, caveat, or question.
Douvdevany et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: