Prismatic slip occurs in polycrystalline titanium diboride after applying 5 to 15 kilobars of hydrostatic pressure. Specimens were subjected to these pressures inside silver chloride matrices by means of a simple cylindrical piston device. The slip was of the type {1010} <1120>. Microhardness indentations produced similar results.