Nano-apatite could be prepared from a homogeneous solution of calcium (Ca)-aspartic acid (Asp) and Ca-glutamic acid (Glu) chelate complex with a high yield. Asp and Glu are components of non-collagenous proteins. Arginine is used to adjust pH to obtain precipitation from a Ca complex solution. Apatite from a Ca- ethylenediaminetetraacetic acid (EDTA) chelate complex was also prepared. These apatites are referred to as Asp-HA, Glu-HA, and EDTA-HA, respectively. Nano-apatite paste was obtained after mixing with water. Synthesized nano-apatite was characterized by X-ray diffraction and Fourier transform infrared measurements. It was revealed that Asp-HA and Glu-HA showed smaller crystal sizes with nano-scale, higher lattice distortion and greater degree of consistency as compared to EDTA-HA. The elution of Ca ion forms Asp-HA and Glu-HA were smaller than that of EDTA-HA. To investigate the influence of the different amino acid ligands for calcium on bone response, bone responses to each nano-apatite paste were evaluated after transplantation into the subperiosteal pocket of the rat calvarial skeleton. Asp-HA and Glu-HA showed greater amounts of new bone formation than EDTA-HA. New bone formation progressed at an especially early stage after implantation with Asp-HA. It is suggested that Asp-HA paste will be useful for bone regeneration.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Waki et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: