This is the authors' abstract. We don't add key points for this paper.
The profiled heat treatment (PHT) method has been used to synthesize MnBi alloys with high-purity low-temperature phase (LTP). In the PHT method, the arc-melted MnBi alloy was remelted then slowly cooled by a pseudo-equilibrium solidification process to promote the formation of LTP phase. The PHT-treated MnBi alloys had an LTP phase up to 94 wt.% and a magnetization of 73 emu/g under a field of 9 T. Scanning electron microscopy showed that there exist some micrometer-sized Mn-rich inclusions in the LTP matrix of the PHT MnBi alloy. The PHT MnBi alloys were crushed into powders with an average size of ~3 μm by low-energy ball milling. These MnBi powders were aligned in an 18 kOe field and warm compacted into a bulk magnet at 300 °C for 30 min. The magnet had a density of 8.2 g/cm3and magnetic properties of Ms= 6.7 kG, Mr= 5.3 kGs, i Hc= 5 kOe, and (BH)max= 6.1 MGOe.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Nguyen et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: