Answers are grounded in this paper and cite their sources.
Preparation of hydroxyapatite (HAP) was investigated by the spray-pyrolysis technique from methanol-water-nitric acid solution of calcium nitrate and phosphoric acid between 800° and 1400°C. The powders obtained consisted of crystalline HAP and a small amount of α-tricalcium phosphate under the experimental conditions used. The content of HAP phase in products increased as the pyrolysis temperature and/or the water content in the solution increased. One phase HAP was obtained by heating the as-prepared powders at 800°C for 1h. Spherical HAP was prepared by this method. The amount of good spherical particles in the powder products increased with increasing Pyrolysis temperature and/or with decreasing water content in the solution. Preparation of HAP with inorganic constituents similar to human bone was also examined. HAP containing Mg, Na, K, Cl and F ions was obtained and it showed good crystallinity.
No takes yet. Share an insight, caveat, or question.
Inoue et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: