Answers are grounded in this paper and cite their sources.
• Combined UV and water effects on various green composites were investigated. • Composite porosity is critical for bulk degradation pathways. • A zigzag pattern was observed in most properties over aging time. • Surface degradation and ablation are mitigated by increased crystallinity. • Composites with Ailanthus altissima exhibit greater durability than PLA. The photochemical degradability of PLA-based composites containing three different natural fillers, namely Posidonia oceanica (PO), Chamaerops humilis (CH), and Ailanthus altissima (AA), was evaluated to understand how the morphological and physicochemical features of these composite systems affect their durability. Composites containing 10% or 20% of filler were prepared by melt-processing and subjected to accelerated weathering involving UV irradiation and condensation cycles. The materials were thoroughly characterized, and the evolution of morphological, physicochemical, and mechanical properties was monitored upon aging time. The results demonstrate the significant impact of filler type on the photochemical stability of PLA-based composites. PO and CH fillers, with high porosity, resulted in less compact composites that underwent rapid hydrolytic degradation, experiencing surface and bulk erosion. AA composites exhibited the highest durability, with their dense morphology effectively delaying degradation. Overall, composites with 10% PO and 20% CH had the lowest stability (less than 6 h), the other PO- and CH-series materials retained durability for 24–30 h, similar to neat PLA, while AA-series composites proved to retain their mechanical properties for up to 36 h.
No takes yet. Share an insight, caveat, or question.
Maio et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: