Highly (117)- and (001)-oriented Bi3.25La0.75Ti3O12 (BLT) thin films were fabricated on Pt/TiO2/SiO2/Si(100) substrates by chemical solution deposition under the appropriate baking and crystallization conditions. The (117)-oriented BLT films exhibited higher remanent polarization (2Pr=24 μC/cm2), than did (001)-oriented BLT films, which exhibited only a slight amount of polarization (2Pr=6.6 μC/cm2). The results of fatigue and retention tests revealed that neither film was fatigued up to 1×1010 switching cycles, and the retained charge was unchanged for 1×104 s.