The presence of a soft zone near the weld interface resulted from the martensite decomposition in the 2.25Cr-1Mo heat-affected zone (HAZ) of a Cr-Mo dissimilar joint during postweld heat treatment (PWHT).In this study, ER90S-B9 filler metal was deposited on 2.25Cr-1Mo (T22) base material and various PWHT durations were applied to investigate the changes in the local structures.Microstructural observations revealed the soft zone formation in the T22 HAZ close to the weld interface.During short PWHT durations, lattice parameters were slightly reduced.The T22 HAZ remained as a martensite structure.The transition period from martensite to ferrite was initiated after 2 h of PWHT.Extreme lattice parameter changes in the soft zone resulted from martensite decomposition and led to the presence of a ferrite band, indicating lower hardness.The decomposition of martensite to ferrite was completed after 4 h of PWHT.From the results, an attempt to apply the x-ray diffraction (XRD) technique was insufficient for differentiating the small changes in local structures.Therefore, the extended x-ray absorption fine structure (EXAFS) technique was introduced to give better analyzed data in terms of rspace.
No takes yet. Share an insight, caveat, or question.
A 2019 study studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: