This is the authors' abstract. We don't add key points for this paper.
An antireflection coating on a polymeric methyl methacrylate substrate is fabricated by poly(allylamine hydrochloride)/poly(acrylic acid) (PAH/PAA) layer by layer deposition method. The authors investigated the effects of acidic treatments of pH 1·8 H2O, pH 2·4 0·05M MgCl2 (NaCl) and different concentrations of PAA on transmissions of the film and resistance to phase separation induced by water and NaCl solution. Different acidic treatments lead to distinct mechanisms of forming nanopores. The optimum of average transmission of the film, 96·86%, at 350–800 nm was obtained using the MgCl2 acidic treatment. The polarised water molecules, Na+ and Cl−, attract polyanions and polycations of PAH/PAA film. Therefore, the resistance to phase separation induced by water and NaCl solution is poor.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: