Answers are grounded in this paper and cite their sources.
Computational study reveals an equiatomic refractory alloy for fusion plasma-facing components, indicating extreme radiation resistance and rapid decay to clearable waste.
The plasma-facing surfaces of a compact spherical-tokamak breeder must keep their strength at high temperature, absorb 14 MeV neutron damage without swelling or embrittling, and decay to a clearable waste class — a combination no legacy plasma-facing alloy meets at once. We report a single radiation-tolerant refractory high-entropy alloy (RHEA), the chromium-free equiatomic W–Ta–V–Ti solid solution, together with the physics that makes it stable and a processing route that makes it manufacturable. The alloy is the survivor of a two-stage screen — a CHGNet machine-learning interatomic-potential pass over 3162 candidate compositions (2853 mechanically admissible), followed by density-functional theory (DFT) confirmation on special quasi-random structures — run on the NVIDIA GPU HPC campaign. A converged variable-cell relaxation gives a formation energy of +0.003 eV/atom: near-neutral, and exactly the signature of an entropy-stabilized single phase. We make that statement quantitative. The configurational entropy of the equiatomic quaternary is =R 4=11.53 J mol^-1K^-1, the atomic-size mismatch is δ=4.1% and the valence-electron concentration is VEC=5.0 — all three inside the empirical single-phase-BCC window — and the entropy-stabilization ratio evaluates to =/||≈ 111, two orders of magnitude above the 1.1 threshold, because the DFT enthalpy is so small. Radiation tolerance is favourable on two independent measures: a helium-bubble rate-theory model gives only 0.024% volumetric swelling at 226 appm He per full-power-year in tungsten (and 0.017% in a ferritic comparator), far below the 1–5% plasma-facing limit and corroborated by a fleet kinetic-Monte-Carlo run; and the heavy-Z, chemically disordered lattice produces few displacements per cascade (52.7 NRT displacements per 15 keV tungsten cascade against 108.8 for iron). A reduced-order elastic screen finds every screened composition Born-stable and ductile (Pugh B/G[1.83,2.22]), and the clean ,Ta,V,Ti,Cr\ palette leaves no isotope with a half-life beyond a century, decaying from ILW^+ at one year to clearable at one hundred. We give a scalable, two-route processing path — vacuum arc melting with thermomechanical processing, or mechanical alloying with spark-plasma sintering — consistent with the demonstrated powder-metallurgy manufacture of fusion-oriented W-based RHEAs. The result is a coherent, computationally grounded, radiation-tolerant plasma-facing alloy with an explicit route from composition to coupon. Key results (frozen anchors): delta = 4.1 %; V = 0.024 %. Methods & codes: OpenMC. Live verification: 10 gate validator(s) with live-recompute cards (7 reproduced, 3 revised). See the Verification section and data/verification.csv. Related: Paper page · De-risking register · 3D model · Learn more about Kronos Part of the 2026 Kronos publication series; independently re-run and stamped in the Kronos de-risking register (DOI 10.5281/zenodo.22645689). All numerical values are frozen design-point anchors; see the register. Public research artifact. No proprietary, financial, or supply-chain information is included.
No takes yet. Share an insight, caveat, or question.
Priyanca Ford (2026) studied this question.