In order to improve the conformity of the glove wearers, the microporous breathable polyethylene gloves are developed using Low-Density Polyethylene (LDPE), Ziegler-Natta Linear-Low Density Polyethylene (ZNLLDPE), Metallocene Linear-Low Density Polyethylene (MLLDPE) and calcium carbonate filler (CC). In this study, LDPE/ZNLLDPE/CC and LDPE/MLLDPE/CC microporous films were prepared to investigate the influence of ZNLLDPE and MLLDPE on the film breathability and elongation. The microporous films were characterized by Scanning Electron Microscope (SEM) analysis, X-ray Diffraction (XRD) analysis and Particulate Filtration Efficiency (PFE) analysis, Water Vapor Transmission Rate (WVTR) testing and mechanical properties testing. Based on the result, LDPE-MLLDPE film yielded film breathability of 335.73 g/m2 ∙ day which is 95.3% higher than LDPE-ZNLLDPE film due to the higher LDPE-MLLDPE film crystallinity and prominent dewetting behaviour between CC and LDPE/MLLDPE matrix. Moreover, the high degree of tie molecules in MLLDPE enabled the film to stretch further upon film elongation. Therefore, LDPE-MLLDPE film showed up to 207.2% comparatively better film elongation than LDPE-ZNLLDPE film. The improved film breathability and film elongation render the mixture of LDPE/MLLDPE/CC as a better material for breathable polyethylene glove production.
No takes yet. Share an insight, caveat, or question.
Tay et al. (2023) studied this question.
Synapse has enriched one closely related paper. Consider it for comparative context: