This is the authors' abstract. We don't add key points for this paper.
Polypropylene (PP) prepared with ethylenebis(4,5,6,7‐tetrahydro‐1‐indenyl)zirconium dichloride in conjunction with methylaluminoxane yields 58 wt.‐% of material insoluble in boiling heptane (C7). The C7‐soluble and the C7‐insoluble fraction exhibit high isotacticity, viz. 97,2% and 98,2%, respectively, relatively narrow molecular weight distribution (weight‐ to number‐average molecular weight M̄w/M̄n = 2,19 for the whole polymer), a small amount of regioirregular units arranged with meso‐placements and relatively low melting points, i.e., 151,3°C for the C7‐soluble and 153,2°C for the C7‐insoluble fraction in spite of high isotacticity.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Tsutsui et al. (1989) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: