This is the authors' abstract. We don't add key points for this paper.
Steady-state creep characteristics in nickel, Ni–Cr and Ni–W alloys were examined in the temperature range 750 to 1000°C and at the stress level from 2.0 to 9.0 kg/mm2. Activation area, A*, obtained from stress-relaxation curves can be correlated to the applied stress, σc, by the equation, A*=A0σc−0.9, where A0 is a constant depending on the solute content, or to the effective stress, σ*, by A*=A0′σ*−0.5, where a constant A0′ is dependent upon the solute content and temperature, T. Internal stress, σi, was obtained from stress-transient dip test as a function of σc and T. The ratio, σi⁄σc, decreases with increasing σc, and T. From these results and characteristic changes in creep curves after a sudden change in σc, it is deduced that Ni–9.5Cr alloy belongs to pure-metal type material. Although the applied-stress exponent is low, the controlling process in the high-temperature creep of Ni–10.3W alloy is also considered to be the same as that in pure-metal type material under the present experimental condition.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Oikawa et al. (1973) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: