Answers are grounded in this paper and cite their sources.
Explosive welding of alternating Grade 1 titanium and AA1050 aluminium sheets produces chemically heterogeneous solidified-melt regions at all interfaces, ranging from large vortex-confined melt zones to ultrathin interfacial layers. These regions contain metastable melt-derived structures with ultrafine-grained or near-amorphous character. Using scanning and transmission electron microscopy combined with synchrotron X-ray diffraction, this study shows that annealing at 903 K transforms these regions into heterogeneous Al 3 Ti reaction layers. Short-term annealing promotes rapid Al 3 Ti formation, whereas annealing for 10 3 h produces a multilayer Ti–Al 3 Ti–Al composite with residual Al and Ti layer thicknesses of approximately 130 and 370 µm, respectively. Al 3 Ti growth is governed by an evolving crystallographic architecture across the reaction zone. Synchrotron X-ray diffraction and local orientation measurements reveal coupled gradients in superstructure, texture, and grain size. Fine-grained regions enriched in Al 48 Ti 16 and Al 24 Ti 8 develop preferentially near the Ti side, whereas coarser regions containing Al 24 Ti 8 and D0 22 -ordered Al 3 Ti form toward the centre and Al side. These findings indicate that long-term Al 3 Ti growth is controlled by transport anisotropy evolving across the layer thickness, rather than by diffusion through a structurally homogeneous intermetallic phase.
No takes yet. Share an insight, caveat, or question.
Puchlerska et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: