Answers are grounded in this paper and cite their sources.
Dimensional accuracy in powder bed 3D printing of concrete is governed by binder distribution, and deviations are direction-dependent. We quantify how the water mass deposited per voxel controls geometric fidelity and deviation anisotropy. Prisms printed with water droplet masses of 29.5 to 63.9 mg per voxel were digitized by high-resolution stereophotogrammetry and aligned with the CAD model. Over this range, the mean deviation of the vertical faces grows from 3.7 to 17.0 mm, the top and bottom faces stay below 6.2 mm, and the print accuracy index rises from 1.13 to 1.59. The apparent flexural modulus (633 to 1078 MPa) and the flexural strength (2.6 to 3.7 MPa) show no clear trend, because excess water diffuses into the surrounding powder and keeps the water-cement ratio at 0.2 to 0.4. A voxel-wise design compensation reduces the mean deviation from 13.5 to 5.5 mm and the maximum from 30.1 to 10.3 mm without post-processing.
No takes yet. Share an insight, caveat, or question.
Wolf et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: