Ring crack initiation loads on glass, using spherical Tungsten carbide (WC) and glass (G) indenters, are measured and analysed. Our measurements demonstrate that environmental humidity plays a key role in determining the load to fracture; experiments conducted without controlling this variable cannot be used to obtain material properties. The role of friction is explicitly considered for dissimilar (WC–G) elastic contacts. For this material pair, the stresses at fracture are well described by a boundary lubrication value of friction coefficient. The fracture loads are used in a fracture-mechanics formulation to calculate crack sizes on glass surfaces. The ‘searched-area’ concept for dissimilar contacts is described, and used to provide crack density values for these surfaces.