Nanoparticles of Eu(3+) doped Y(2)O(3) (core) and Eu(3+) doped Y(2)O(3) covered with Y(2)O(3) shell (core-shell) are prepared by urea hydrolysis for 3 h in ethylene glycol medium at a relatively low temperature of 140 °C, followed by heating at 500 and 900 °C. Particle sizes determined from x-ray diffraction and transmission electron microscopic studies are 11 and 18 nm for 500 and 900 °C heated samples respectively. Based on the luminescence studies of 500 and 900 °C heated samples, it is confirmed that there is no particle size effect on the peak positions of Eu(3+) emission, and optimum luminescence intensity is observed from the nanoparticles with a Eu(3+) concentration of 4-5 at.%. A luminescence study establishes that the Eu(3+) environment in amorphous Y (OH)(3) is different from that in crystalline Y(2)O(3). For a fixed concentration of Eu(3+) doping, there is a reduction in Eu(3+) emission intensity for core-shell nanoparticles compared to that of core nanoparticles, and this has been attributed to the concentration dilution effect. Energy transfer from the host to Eu(3+) increases with increase of crystallinity.
No takes yet. Share an insight, caveat, or question.
Singh et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: