Alumina ( Al_2{O_3} ) addition in 3mol% yttria-stabilised tetragonal zirconia polycrystals (3Y-TZP) enhances dental ceramics’ mechanical properties and microstructure. This study examines the effects of 0, 0.03, 0.06 and 0.09wt.% Al_2{O_3} addition on Vickers indentation fracture resistance (KIFR) mode I fracture toughness (KIC) and other mechanical characteristics of 3Y-TZP ceramics. The results show that 0.06wt.% Al_2{O_3} improves relative density, Young’s modulus, Vickers hardness, KIFR and KIC by less than 8%. With higher Al_2{O_3} content, grain size tends to be reduced. Consistent KIFR trends across various Vickers equations indicate unreliable correlations, with more than 32% discrepancy between KIFR and KIC values from Vickers indentation and Single Edge Laser Notch Beam (SELNB) methods.