Assuming a geometrical model with mutual (H‐H) blocking, for hydrogen dissolved in titanium and titanium alloys experimental data are compared. It is found that interstitial sites with pure titanium coordination only host hydrogen atoms. In alloys with bcc crystal lattices only tetrahedral interstitial sites are occupied, whereas in hep alloys both tetrahedral and octahedral interstitials host hydrogen. A linear relation is found which connects the partial molar absorption enthalpy ΔHOHand the partial molar excess absorption entropy ΔSE, OHat infinite dilution of dissolved hydrogen. The enthalpy of absorption ΔHOHcan be rationalized as a function of interstitial hole size and an optimum hole radius of 47 pm is found for titanium and titanium alloys.