Answers are grounded in this paper and cite their sources.
Thin films of TiS2 and TiS3 have been prepared by thermal chemical vapor deposition by reacting TiCl4 and a series of sulfur sources [hexamethyldisilthiane ((CH3)3SiSSi(CH3)3), t-butyl sulfide ((CH3)3CSC(CH3)3), and t-butyl disulfide ((CH3)3CSSC(CH3)3)]. Thin films of TiS3 were prepared by reacting TiCl4 and TBDS at a deposition temperature less than 260°C. As the deposition temperature was increased, TiS2 also formed within the deposited film, until at temperatures greater than 400°C only TiS2 was formed. The use of the other sulfurizing sources resulted in the deposition of only TiS2 throughout the temperature range studied (200–550°C). The morphology of the TiS2 films varied remarkably with deposition temperature. At low temperatures the films were very dense and X-ray diffraction indicated that the films were deposited preferentially with the crystallographic “c” axis perpendicular to the substrate. As the temperature increased above 300°C, a porous honeycomb structure was deposited with the crystallographic “c” axis parallel to the substrate.
No takes yet. Share an insight, caveat, or question.
Chang et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: