Answers are grounded in this paper and cite their sources.
Constant strain-rate compression tests on ice single crystals at temperatures between –20°C and -0.2°C are described. The power-law dependence of yield stress on strain-rate gives a value of n which varies from 1.95±0.04 at –0.2°C to 2.07±0.08 at –20°C. The activation energy of deformation varies with strain-rate, but a mean value of 70±2 kJ mol –1 is obtained, with no indication of any increase close to maleting point,as has been found polycrystalline ice. An apparent work-hardening effect, at strains greater than 15%, is explained as being due to bending of the crystal changing the orientation of the basal planes.
No takes yet. Share an insight, caveat, or question.
Jones et al. (1978) studied this question.