Answers are grounded in this paper and cite their sources.
Multi-component (AlCrTaTiZr)–Si x –N films were deposited on silicon wafers by reactive RF magnetron co-sputtering. The effect of silicon content on the structure, morphology and mechanical properties of the nitride films was investigated. Nitride films with lower silicon content remained as a simple NaCl-type face-centred cubic (FCC) structure. As the silicon content reached 7.9 at%, thermodynamically driven phase separation occurred, leading to a nanocomposite structure consisting of an FCC solid-solution nitride and an amorphous SiN x phase. These nitride films exhibited a high hardness of 34 GPa and remained at a constant level up to 7.9 at% Si. The reduced hardness at a silicon content of 10.2 at% was attributed to the appreciable amounts of softer amorphous segregation. The silicon incorporation significantly improved the oxidation resistance of (AlCrTaTiZr)N films. The film containing 7.9 at% Si annealed at 1000 °C for 2 h in air only had a 330 nm-thick oxide layer. The optimum Si content is 7.9 at% since it gives the best combination of hardness and oxidation resistance.
No takes yet. Share an insight, caveat, or question.
Cheng et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: