Submonolayer dissolution of platinum (Pt) nanoparticles under potential cycling is specified by a channel flow double electrode system. Dissolution of Pt 2+ starts at 0.6 V (vs. standard hydrogen electrode) in an anodic scan. The amount of dissolved Pt 2+ below 1.0 V was calculated using collector current ( I C ) and was confirmed by ex-situ inductively coupled plasma mass spectrometry. The amount of Pt 2+ and Pt 4+ dissolved in different potential regions during potential cycling was quantified by I C for the first time. A mechanism of Pt dissolution under potential cycling in 0.5 M H 2 SO 4 was proposed, and an in-situ system capable of quantitatively monitoring submonolayer dissolution of Pt 2+ and Pt 4+ was established.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2014) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: