Answers are grounded in this paper and cite their sources.
We used phonon frequency shift measured by Raman scattering to determine the strain depth profile within an epitaxial layer of a mismatched heterolayer as its thickness increases beyond the critical one. Three different modes of operation were examined to confirm the results: (i) low penetration laser used to probe strained layers of different thicknesses; (ii) changing the laser wavelength and thereby the light penetration depth inside a given thick strained layer; (iii) disorder induced Raman scattering in a forbidden polarization configuration. It is found that in the case of In0.40Ga0.60As/GaAs, a relaxation of strain is taken place in quantized thickness steps, preserving the higher strain of layers closer to the interface. It is inferred that the structural defects formed as thickness exceeds the critical one, are generated at the surface, are localized there and affect the strain and thereby the lattice parameter of the successive growth. This procedure repeats itself in steps, these steps are even better viewed at the forbidden configuration, where the scattering is disorder induced. We show the advantage gained in cleaving the sample and microprobing it parallel to the interface, a method by which one measures directly the phonon frequency versus the distance from the interface. In addition, the interface can be studied with much greater detail through a second order Raman scattering steming from zone boundary, for which the phonon wavelength is of the order of 1 nm. This is demonstrated on ZnSe/GaAs, where small islands of extremely high strain were found. These could not be detected by first order scattering because the phonon wavelength is very large.
No takes yet. Share an insight, caveat, or question.
O. Brafman (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: