Answers are grounded in this paper and cite their sources.
The long-term confusing glass transition temperature, T g, and specific heat capacity, Δ C p, of the 4,4‘-diisocyanatodiphenylmethane (MDI) and 1,4-butanediol (BD) hard segment in segment polyurethanes have been clearly evidenced by using a new series of completely phase-mixed polyurethanes while being extrapolated to 100% hard segment content. The hard segment T g and Δ C p thus obtained are 108 °C and 0.38 J/g °C, respectively, which are equivalent to the reported Tg and Δ C p of a high molecular weight MDI−BD homopolymer. In addition, if a single homogeneous phase is present, the observed Δ C p and T g are found to be given by the linear weighted combination of the pure constituent values. This provides a simple relationship to access the composition of the individual microdomain in segment polyurethanes, providing that the phase-separate morphology does not affect the microdomain glass transition behavior.
No takes yet. Share an insight, caveat, or question.
Chen et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: