Herein, a novel green emitting long-persistent Sr3SiAl4O11:Eu2+/Dy3+ phosphor was synthesized in a single phase form using facile solid state reaction method under the reducing atmosphere of 10% H2 and 90% N2. The resulting phosphor exhibits hyper-sensitive strong broad green emission, peaking at 510 nm upon 340 nm excitation wavelength, which is attributed to the 4f65d1-4f7 transitions of emission center of europium (Eu2+) ions. Moreover, the incorporation of dysprosium (Dy3+) ions, which act as effective hole trap centers with appropriate depth, largely enhances the photoluminescence characteristics and greatly improves the persistent intense luminescence behavior of Sr3SiAl4O11:Eu2+/Dy3+ phosphor under ultraviolet (UV) excitation. In addition, with the optimum doping concentration and sufficient UV excitation time period, the as-synthesized phosphor can be persisted afterglow for time duration ∼4 h with maximum luminescence intensity. Thus, these results suggest that this phosphor could be expected as an ultimate choice for next generation advanced luminescent materials in security applications such as latent finger-marks detection, photo-masking induced phosphorescent images, and security code detection.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Gupta et al. (2015) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: