Single‐phase, cubic solid solutions of baseline composition 25% Y 2 O 3 —75% Bi 2 O 3 with and without aliovalent dopants were fabricated by pressureless sintering of powder compacts. CaO, SrO, ZrO 2 , or ThO 2 was added as an aliovalent dopant. Sintered samples were annealed between 600° and 650°C for up to 4000 h. Samples doped with ZrO 2 or ThO 2 remained cubic, depending upon the dopant concentration, even after long‐term annealing. By contrast, undoped, CaO‐doped, and SrO‐doped samples transformed to the low‐temperature, rhombohedral phase within ∼ 200 h. Conductivity measurements showed no degradation of conductivity in samples that did not undergo the transformation. In samples that underwent the transformation, a substantial decrease in conductivity occurred. The enhanced stability of the ZrO 2 ‐ and ThO 2 ‐doped samples is rationalized on the basis of suppressed interdiffusion on the cation sublattice.
No takes yet. Share an insight, caveat, or question.
Fung et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: