The strength σy(D) of a polycrystal can decrease or increase with the grain diameter D, i.e., the famous Hall-Petch (HP) and inverse-Hall-Petch (IHP) behaviors, respectively. However, σy(D) under thick grain boundaries (GBs) (i.e., GB thickness $l>1$ particle) and σy(l) have rarely been explored. Here we measure them by systematically varying D and l of two-dimensional glass-crystal composites in simulations. We demonstrate that increasing l and decreasing D have similar effects on reducing dislocation motions and promoting GB deformations. Consequently, the classical HP-IHP behaviors of σy(D,l=1) and our generalized HP-IHP behaviors of σy(D,l) share similar mechanisms and can be unified as σy (AGB/Aₜot), where AGB/Aₜot is the fraction of the amorphous region. The results reveal a way to exceed the maximum strength of normal polycrystals. The generalized HP-IHP behaviors of σy(D,l) should be similar in 2D and 3D, except that the HP effect in 3D is stronger.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Xu et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: