Answers are grounded in this paper and cite their sources.
Composites of ZrB 2 –SiC-WC for hypersonic flight applications require the presence of a B 2 O 3 –SiO 2 -based surface layer covering a dense ZrO 2 scale to suppress high-temperature oxidation. Previously, we showed that the addition of 3.6 vol % WC to ZrB 2 -20 vol % SiC enhances the stability of the composite at 1800 °C. Stabilization was mainly due to densification of the underlying ZrO 2 scale. In this article, we ask whether increasing the SiC content can extend this stability? We increased the SiC content to 30% and determined whether the extra SiO 2 formed during SiC oxidation can provide additional protection up to 2000 °C. Composites of ZrB 2 -30 vol % SiC-3 vol % WC were fabricated by SPS at 1950 °C and tested at various oxidation conditions. Non-WC-containing samples (Z30S) show significant surface degradation in air at 1800 °C, loss of protective B 2 O 3 –SiO 2 -based surface layers, and a thick porous ZrO 2 scale that allows for oxygen penetration. WC-containing samples (Z30SW) preserve protective layers under the same conditions, with dense ZrO 2 and B 2 O 3 –SiO 2 -based surface layers, thicker than those for Z30S and compositions previously studied. Following the exposure to air at 1800 °C for 15 min, Z30S and Z30SW lost 1.51 ± 0.18 mg cm –2 and gained 1.96 ± 0.08 mg cm –2, respectively. After 15 min at 2000 °C and low pO 2 (∼10 –6 Pa), samples undergo active oxidation of SiC and loss of the SiO 2 -based surface layer. A ZrO 2 layer does not form under these low pO 2 conditions; thus, a highly porous ZrB 2 skeleton is formed at the surface, leading to a damaged Z30S surface layer that is 40 μm thick. In the Z30SW samples, the ZrB 2 skeleton is 30% thinner, intact, and much denser, allowing significantly less oxygen to reach the base composite.
No takes yet. Share an insight, caveat, or question.
Nussbaum et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: