Answers are grounded in this paper and cite their sources.
The tested steels were cooled to room temperature using different cooling paths after two-stage rolling, and effects of cooling paths on microstructure, mechanical properties and precipitation behaviors of Nb-Ti micro-alloyed steels were investigated.The results show the hot rolled plates with fine grain were produced at the cooling path of ultra fast cooling + air cooling, and the average grain size, lower yield strength and ultimate tensile strength are about 7.76 μm, 425 MPa and 500 MPa, respectively.The fine precipitation particles ranging from 2 nm to 7 nm were observed in the samples cooling with ultra fast cooling + furnace cooling, but are only a few globular precipitates in the samples cooling with ultra fast cooling + air cooling.The inter-phase precipitation was observed in samples cooling with air cooling after finish rolling.These plates with different cooling paths were annealed at 700 for 300 s.The precipitation particles were obviously coarsened during annealing.It can be found that the average grain size of the samples with cooling path of ultra fast cooling + furnace cooling is 6.47 μm and the increments of lower yield strength and ultimate tensile strength are about 50 and 30 MPa, respectively.The strength increment mainly depends on fine grain * "#-.N110607003 N100507002 .
No takes yet. Share an insight, caveat, or question.
Chen et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: