The aim was to evaluate the effect of different zirconia discontinuous fiber fractions on radiopacity and other selected properties of glass discontinuous fiber-reinforced flowable composite (Exp-SFRC). Exp-SFRC was prepared by mixing 30 wt% of resin-matrix and 45 wt% of particulate-fillers to 25 wt% of various weight-fractions of E-glass/zirconia discontinuous fiber-fillers (25:0, 20:5, 15:10, 10:15, 0:25 wt%). Flexural strength and fracture toughness were determined for each experimental material. Radiograph of each Exp-SFRC and aluminium step wedge were taken to determine the radiopacity. Degree of conversion and light-transmission were also measured. Scanning electron microscopy was used to evaluate the microstructure of the Exp-SFRC. Analysis of variance (ANOVA) revealed that fractions of E-glass/zirconia discontinuous fiber-fillers had significant effect (p<0.05) on radiopacity and other tested properties of the Exp-SFRCs. Replacing low fraction of E-glass fiber with zirconia fiber-fillers can increase the radiopacity of the fiber-reinforced composite without deteriorating the mechanical properties, although, degree of conversion was decreased.
No takes yet. Share an insight, caveat, or question.
Garoushi et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: