A two-stage roasting and leaching process was developed to maximise vanadium recovery from vanadiferous titanomagnetite (VTM) concentrate while reducing residual sodium to levels compatible with direct reduced iron (DRI) feedstock. Critical parameters, such as roasting temperature, soda ash dosage, roasting and leaching durations, slurry concentration, and leaching temperature, were systematically optimised using a central composite design (CCD) approach based on response surface methodology (RSM). The optimised parameters not only achieved vanadium recoveries exceeding 90% but also reduced the sodium content to 0.31 wt%. A subsequent mild acid leaching step reduced sodium further to 0.071 wt%, which meets the stringent DRI-grade pellet requirements. Kinetic studies suggested a first-order, surface-reaction-controlled leaching mechanism for vanadium with an activation energy of 43.2 kJ/mol. To meet the DRI and steelmaking process requirements, this work offers a feasible and scalable solution for the sustainable extraction of vanadium while addressing sodium contamination.
No takes yet. Share an insight, caveat, or question.
Golpayegani et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: