X-ray diffraction intensities were measured from a BeO single crystal with wurtzite structure specially treated to reduce extinction effects. Preliminary least-squares refinement yielded experimental structure factors on an absolute scale, corrected for extinction and anomalous dispersion, and a reference model Be2+O2- with position parameter z = 0.3778 (4) and anisotropic Debye-Waller factors corresponding to atomic mean-square displacements with spherical average (u2) = 0.0045 (3) and 0.00353 (1) Å2 and prolateness (u23) - (u2) = 0.0008 (4) and 0.00005 (9) Å2 for Be2+ and O2-, respectively. The residual differences Fo- Fc (of these experimental structure factors and those of the reference model) were analysed in terms of site-symmetrized multipole expansions. The phases of Fo were refined iteratively to take into account the effect of the significant multipole components found. The contribution of the Be2+ ion was subtracted to make possible a study of the oxygen lattice. Significant multipole components of third, fourth and sixth order indicate that the oxygen in BeO forms bonded hexagonal O2- planes. They build up diffuse O-O bridges strongly bent towards the stabilizing Be2+ ions above the plane. The Be2+ ions exhibit a stretching quadrupole-like deformation suggesting some covalency of the bonding they build between the O2- planes. There is some evidence of anharmonicity of atomic vibrations, particularly in the direction of the hexagonal axis.
No takes yet. Share an insight, caveat, or question.
Vidal-Valat et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: