Answers are grounded in this paper and cite their sources.
NIR‐sensitized (NIR=near‐infrared) radical photopolymerization can be employed to chemically cure VOC‐free coatings; that is, either a powder coating or liquid monomer coating system with no significant components of volatile organic compounds (VOC). A NIR laser with line‐shaped focus was applied to cure the coatings. This system operated in multi‐wavelength mode where preferentially the emission wavelengths λ=808 nm and 980 nm of the laser system could be employed to solidify and crosslink the starting components as a transparent film; that is, chemical drying by photonic events. Cyanines absorbing at λ=980 nm and 808 nm functioned as heat generators to melt the powder and as sensitizers (Sens) to generate initiating radicals in combination with a radical initiator (RI). The radical initiator was either the iodonium salt RI‐1 ([(t‐C4H9‐Ph)2I+][(CF3SO2)2N−]) or triazine A (RI‐2). Photoinduced electron transfer between the excited states of Sens and RI was found to control the efficiency of initiating radicals. Line‐shape‐focused laser experiments demonstrated that both liquid VOC‐free coatings and solid powder coatings can be cured. Curing of solid powder coatings occurs with a curing rate of 3.6 m min−1, opening the possibility to introduce NIR laser curing as a new technology in coating sciences. Finally, rheological measurements and differential scanning calorimetry (DSC) were applied to characterize the flow properties of the molten powder and the glass transition temperatures of the crosslinked materials, respectively. The molten powder coating behaved like a liquid up to 160 °C as concluded from the complex shear modulus (G*), while the phase shift (∂) documents crosslinking above this temperature.
No takes yet. Share an insight, caveat, or question.
Schmitz et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: