Answers are grounded in this paper and cite their sources.
The use of transient glass‐phase processing to lower the glass‐melting temperature and subsequent heat‐treatment temperature of stoichiometric SrAl 2 Si 2 O 8 to produce the stable monoclinic form has been described. Two nonstoichiometric, low‐melting, alumina‐deficient, strontium aluminosilicate compositions were melted, quenched, and milled into glass powders. B 2 O 3 was dissolved into one of the glass compositions to control the crystallization behavior. The glass powders were then wet‐mixed with enough alpha‐Al 2 O 3 powder so that the overall composition was that of stoichiometric SrAl 2 Si 2 O 8 (B 2 O 3 neglected). The four compositions were dry‐pressed into pellets and sintered in three processes. Glass‐alumina pellets with dissolved B 2 O 3 were densified via viscous‐phase sintering at 1100°C, followed by complete dissolution of the alumina and crystallization to ~100% monoclinic SrAl 2 Si 2 O 8 . Pellets without dissolved B 2 O 3 required considerably higher temperatures to form ~100% monoclinic SrAl 2 Si 2 O 8 in a modified process.
No takes yet. Share an insight, caveat, or question.
Chinn et al. (1998) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: