A series of hyperbranched poly(ferrocenylenesilyne)s, [(η 5 -C 5 H 4 ) 2 FeSi(R)] n {R = CH 3 [ 1 (1)], CH CH 2 [ 1 (V)], n -C 8 H 17 [ 1 (8)], n -C 12 H 25 [ 1 (12)], n -C 16 H 33 [ 1 (16)], n -C 18 H 37 [ 1 (18)]}, was prepared in good isolation yields (up to 77 wt %) by one-pot coupling reactions of dilithioferrocene with trichlorosilanes. While the polymers with small R groups [ 1 (1) and 1 (V)] were partially soluble, those with long alkyl chains [ 1 ( m ) with m ≥ 8] were completely soluble and readily film forming. The polymers exhibited diagnostic solution properties of hyperbranched macromolecules; for example, 1 (18) had a high absolute molecular weight ( M w = 5 × 10 5 Da) but a low intrinsic viscosity ([ η ] = 0.02 dL/g). Spectroscopic analyses revealed that the polymers possessed rigid skeleton structures with extended conjugations, with their absorption spectra tailed into the infrared region (>700 nm). With an increase in the alkyl chain length, the polymer changed from glassy to rubbery state. The polymers lost little of their weights when heated to ∼400 °C but ceramized when pyrolyzed at higher temperatures, with ceramization yield increasing with a decrease in the alkyl chain length. Sintering 1 (1) and 1 (V) in 700−1200 °C produced ceramics in ∼50% yields. Higher temperature pyrolyses favored the formation of ceramics with bigger inorganic nanoclusters and better magnetic performances. The ceramic prepared from the calcination of 1 (1) at 1200 °C contained large iron silicide nanocrystals and exhibited high magnetizability (up to ∼51 emu/g) but near-zero remanence and coercivity. This ceramic is thus an outstanding soft ferromagnet with a high magnetic susceptibility and practically nil hysteresis loss.
No takes yet. Share an insight, caveat, or question.
Sun et al. (2003) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: