This is the authors' abstract. We don't add key points for this paper.
Summary The issues of short thickening time of geopolymer at higher temperature conditions are significant barriers to broader application. In this study, the effects of raw material proportions and additives (activators, retarders, and fluid loss agents) on the performance of metakaolin (MK)-fly ash (FA)-based geopolymer under conditions of 70°C were investigated, and the effect mechanism of retarders was analyzed. The results indicate that when sodium silicate is combined with sodium hydroxide, the geopolymer exhibits high strength. Specifically, when the FA/MK ratio is 6:4 and the water/solid ratio is 0.7, the geopolymer exhibits high strength and favorable rheological properties. The addition of 0.9% barium chloride dihydrate (BaCl2·2H2O), 4% zinc sulfate heptahydrate (ZnSO4·7H2O), 10% ethylene glycol (EG), or 10% ethylenediaminetetraacetic acid disodium salt (EDTA-2Na) significantly increases the setting time, but this adversely affects the strength. This occurs primarily due to the products formed from the reaction between the retarder components and water glass or mineral components, which cover the surface of the raw materials and reduce the reaction rate. When utilizing a combined dosage of 0.9% barium chloride dihydrate (BaCl2·2H2O) and zinc sulfate heptahydrate (ZnSO4·7H2O) as a retarder, the thickening time of the geopolymer significantly increases. Furthermore, the addition of 0.5% carboxymethylcellulose sodium (CMC-Na) effectively controls water loss, with the initial setting time exceeding 45 minutes and strength of up to 8 MPa, demonstrating satisfactory settlement stability, but it adversely affects rheological properties.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: