Answers are grounded in this paper and cite their sources.
This study investigates the corrosion resistance of two-layer Gd 2 Zr 2 O 7 /YSZ, three-layer dense Gd 2 Zr 2 O 7 / Gd 2 Zr 2 O 7 /YSZ, and a reference single-layer YSZ coating with a similar overall top coat thickness of 300-320 µm. All the coatings were manufactured by suspension plasma spraying resulting in a columnar structure except for the dense layer. Corrosion tests were conducted at 900 °C for 8 h using V 2 O 5 and Na 2 SO 4 as corrosive salts at a concentration of approximately 4 mg/cm 2 . SEM investigations after the corrosion tests show that Gd 2 Zr 2 O 7 -based coatings exhibited lower reactivity with the corrosive salts and the formation of gadolinium vanadate (GdVO 4 ), accompanied by the phase transformation of zirconia was observed. It is believed that the GdVO 4 formation between the columns reduced the strain tolerance of the coating and also due to the fact that Gd 2 Zr 2 O 7 has a lower fracture toughness value made it more susceptible to corrosion-induced damage. Furthermore, the presence of a relatively dense layer of Gd 2 Zr 2 O 7 on the top did not improve in reducing the corrosion-induced damage. For the reference YSZ coating, the observed corrosion-induced damage was lower probably due to combination of more limited salt penetration, the SPS microstructure and superior fracture toughness of YSZ.
No takes yet. Share an insight, caveat, or question.
Jonnalagadda et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: