When polymerization of propene was conducted using the C 2 -symmetrical zirconocenes rac -Et(2,4,7-Me 3 Ind) 2 ZrCl 2 ( I ) and rac -Me 2 Si(2-Me-4-Ph-Ind) 2 ZrCl 2 ( II ) combined with Ph 3 CB(C 6 F 5 ) 4, the isotacticity ([mmmm]) and the melting point ( T m ) of the produced polymer markedly increased, along with a decrease of the polymerization temperature from 30 to −78 °C. Thus, isotactic polypropene (iPP) with T m = 168.9 °C was obtained from the polymerization with catalyst I at −78 °C, whereas the [mmmm] and T m of iPP were almost unchanged in the same temperature range when the C 1 -symmetrical zirconocene iPr(3-tBuCp)(3-tBuInd)ZrCl 2 ( III or III ‘) was employed.