Answers are grounded in this paper and cite their sources.
We present a facile, broadly applicable method to prepare nanoporous silver films using soluble salt nanoparticles as pore templates. The fabrication starts by printing a silver/CaCO 3 nanoparticle based ink onto a flexible substrate and removing the CaCO 3 by washing in a weak acid. The membrane thickness and pore size can easily be tuned between 0.5−5 μm and 30−300 nm, respectively, by a simple pH or temperature treatment (sintering at 200 °C). As a conceptual demonstration of the resulting large-area, defect-free, and homogeneous microstructure, we use these membranes to efficiently filter aqueous dispersions of carbon nanoparticles (20 nm primary particle size) at a filtration efficiency of >99.6%.
No takes yet. Share an insight, caveat, or question.
Luechinger et al. (2010) studied this question.