Laser-induced damage to the final reflective and diffractive optics limits the total output energy of petawatt laser systems with pulse durations ranging from a few hundred femtoseconds (fs) up to a few tens of picoseconds (ps). In this study, the laser damage to HfO 2 /SiO 2 and Ta 2 O 5 /SiO 2 multilayer dielectric high-reflectivity (HR) coatings induced by a 1053 nm laser with a pulse width of 8.6 ps was studied to investigate the nano-absorbing precursors in ps regimes. The HfO 2 /SiO 2 HR coating exhibited stronger laser resistance than the Ta 2 O 5 /SiO 2 HR coating. Flat-bottom pits, pinpoints, and funnel pits were the three typical damage morphologies for the experimental HR coatings. The damage to the HfO 2 /SiO 2 HR coating was primarily dominated by flat-bottom pits, whereas dense pinpoints were the most significant damage for the Ta 2 O 5 /SiO 2 HR coating. The nano-absorbing precursors introduced by the ion-assisted deposition process were proved to be the damage precursors that trigger pinpoints under a strong electric field intensity (EFI). The nano-absorbing precursors located in the second EFI peak of the SiO 2 top layer induced the funnel pits. The funnel pits were expected to be the previous stage of the flat-bottom pits. After they grew along the upward-sloping crack and separated from the interface, the flat-bottom pits were formed. In addition, poor-binding interfaces promoted the formation of flat-bottom pits.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Gong et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: