Catalytic performance depends largely on the surface properties. Here, the surface phase composition of iron molybdate catalysts with different Mo/Fe atomic ratios calcined at different temperatures was studied by UV Raman spectroscopy. In this study, the surface enrichment of MoO 3 that the Mo-rich catalysts undergo during calcination treatment is revealed by the increase in the Raman intensity of MoO 3 . X-ray photoelectron spectroscopy (XPS) analysis provides further evidence that the concentration of Mo increases evidently with increasing calcination temperature. The surface enrichment of MoO 3 also results in a significant variation of the morphologic appearance as evidenced by the presence of a needle-like material assigned to MoO 3 on the surface, while the surface phase composition remains almost unchangeable for the sample with a stoichiometric atomic ratio. These results are attributable to the formation of a substitution structure of Fe 3+ ions in an octahedral coordination by Mo 6+ ions in Mo-rich catalysts, and MoO 3 is easier to segregate from such a structure as a second phase concentrated on the surface.
No takes yet. Share an insight, caveat, or question.
Xu et al. (2008) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: