Answers are grounded in this paper and cite their sources.
A lightweight and stiff composite metal foam was developed using LM24 alloy (an aluminium alloy with major compositions of 11.7%Si, 4%Cu, 1.8%Zn, 1%Fe, 0.5%Mg, 0.1%Ni and 80.9%Al) as a matrix material and Cermet Hollow Spheres (CHS) of diameter range 3–6 mm as pore-creating agents, for higher energy absorption applications such as blast mitigation. The CHS were used for further performance improvement of the foam developed earlier by using Steel Hollow Spheres (SHS) as reinforcement in the aluminium matrix. The CHS were fabricated from a blend of silicon carbide (SiC) and stainless steel (SS316L) powders by powder metallurgy technique. A comparative study was thus performed for better compressive strength, high porosity, low density and high energy absorption capacity. The foam samples were prepared at 750°C by stirring and gravity casting after mixing the CHS in the melt. The energy absorption capacity of the foam was found to be 87.46 MJ/m3, which is higher than the foam previously developed with SS316L hollow spheres as reinforcements, which had a capacity of about 51 MJ/m3.
No takes yet. Share an insight, caveat, or question.
Zewdie et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: